Ultrasonic welding offers several advantages over traditional welding and crimping methods:
- Maintains Conductor Integrity: Unlike traditional methods, ultrasonic welding does not melt conductor materials, preserving their integrity.
- High Electrical Conductivity: It ensures high electrical conductivity with very low resistance.
- Clean and Efficient: The process generates no sparks, fumes, or residual solder.
- Fast Welding: It provides a quick welding time without residual solder or other contaminants.
Standards and Testing Methods

After ultrasonic welding, joints undergo several tests to ensure their strength and reliability.
Torsion Force Standards and Testing Methods

Tear Force Standards
Tear force is the maximum force required to disengage conductors at welded joints, measured in Newtons (N). Automotive wire harnesses in China follow the QC/T 29106-2014 standard, which specifies tear force requirements for solderless welding methods. This standard ensures that joints maintain their strength in various conditions.
Testing Methods

Tear force tests use a tensile testing machine. The load range should be set according to specific requirements, with an error margin of no more than ±1%. The clamps should move at a uniform speed, typically between 20 and 200 mm/min. In this research, tests were conducted at 100 mm/min, a standard speed for most manufacturers.
A sample is secured in the machine and aligned along its wire axis. Tension is applied, and the maximum force (F) recorded during extraction.
Factors Affecting Joint Tear Force
Several factors influence the tear force of automotive wire harness joints after ultrasonic welding:
Key Welding Process Parameters
Key parameters include amplitude, width, welding energy, and air pressure. Deviations from acceptable ranges can lead to inadequate tear force or overheating. Extensive testing is necessary to find optimal settings.

Table 2 provides welding process parameters based on experimental data for various cross-sectional areas of wire harnesses. Cooling with compressed air is crucial to maintain welding quality.
Conductor Arrangement
The arrangement of conductors during welding impacts the quality. For example, Volvo's wire harnesses use a specific 1+2 arrangement for optimal results. Tests on different arrangements showed varying tear force outcomes.
Table 3 illustrates the results for different conductor arrangements, showing that arrangement 'c' yields the best results.
Treatment of Conductor Surface Attachments
Contaminants on conductor surfaces, such as oil, oxidation, or impurities, can affect welding quality.
- Residue Lubricants: Maintain lubricant concentrations within recommended limits to prevent oxidation and residue buildup.
- Oxidation: Use anti-oxidation measures to prevent reduced tear force due to copper oxide layers.
- Plastic Exudates: Adhere to a first-in, first-out policy for storage to avoid reduced welding quality due to exudates.

Conclusion
Ultrasonic welding outperforms traditional methods like crimping and soldering by eliminating high contact resistance, flux, and fumes. Although it requires stringent control over welding parameters and conductor treatment, it offers superior conductivity and efficiency. Continued research and practice will enhance its use in the automotive wire harness industry.